Product Details:
|
Fiber Type: | PP Twisted Bunchy Form | Application: | Reinforce The Cement Concrete And Industrial Floor |
---|---|---|---|
Raw Material: | Polypropylene | Break Strength: | 560MPa Min |
Length: | 54mm | Break Tensile Ratio(%): | 15Mpa Min |
High Light: | Polypropylene Macro Synthetic Fiber,54mm Macro Synthetic Fibers Concrete,Macro Synthetic Fiber 54mm |
PP Fiber Twisted Bunchy form
Product Description
Polypropylene Fiber (PP Fiber) is made from 100% virgin PP granular, after extruding from different mould and technology, we can get 4 different types of fiber, including Monofilament form, Fibrillated Mesh form, Twisted Bunchy and Wave form with different size. These fiber can improve the reinforcement of mortar or concrete performance effectively to make them strong and protect the projects.
1. This fibre is used to instead of steel fiber for reinforcement to cement concrete. Compared with steel fiber, it has the advantage of easy dispersing and blending, no damage to the mixing equipments, etc
APPLYING INSTRUCTION:
1. Ration design of the fibre concrete:
Generally the recommended amount to add to the concrete is more than 2.7kg per sqm (volume ratio is 0.3%), reinforcement adding amount is
5.5kg, Compared with adding 47kg of steel fibre, 5.4kg polymer fibre has the same volume ratio to the concrete.
2. Length: 40mm, 54mm for common crack-resistant requirement.
3. Matching Ratio:
Usually, it is no need to Change the matching ratio of the concrete. Considering the requirement of fissure-resistant, the polymer fiber is recommend to combine with the PP fiber mesh form with the volume ratio of 1:1(0.9kg fiber-mesh to per sqm of cement concrete). .
4. Mixer Adoption:
Double-axle horizontal compelling mixer is priority.
5. Mixing process:
Crushed stones, fibers and sands are put into the mixer in succession. After stirring for two minutes, fiber will fully spread and then add cement and water and stir normally. The addition of materials also can be put into as common concrete, but the stirring time should be properly prolonged to make fiber com-pletely mixed.
6. Shaping & Maintenance:
There is no special requirement, may along the vibrating time for 30s, The maintenance of the fibre concrete should be done same as the normal
concrete.
Specification
Raw material | PP+PE |
Modulus (Mpa) | 5000min |
Fiber Length (mm) | 54 |
Density | 0.91g/cm3 |
fiber diamter | 0.3±0.05 |
acid&alkali resistance | Excellent |
Break tensile ratio | 15%min |
Break strength (Mpa) | 560min. |
Application:
1. The surface of road, bridge, runway and floor of the factory.
2. concrete reinforcement, industrial floor
Packing
1kgs per bag, 10kgs per carton.
Quantity: 400CTNS/20`FCL;
828CTNS/40`FCL;
930CTNS/40`HQ
or
500g, or 1kg net per PE bag
10kgs per plastic woven bag
5000kgs/1X20`FCL without pallet
13000kgs/1X40`HC without pallet
Packing image: